Standard Test Method for Oxidative-Induction Time of Polyolefins by Differential Scanning CalorimetryD3895-14ASTM|D3895-14|en-USStandard Test Method for Oxidative-Induction Time of Polyolefins by Differential Scanning CalorimetryStandardD3895 Standard Test Method for Oxidative-Induction Time of Polyolefins by Differential Scanning Calorimetry>newBOS Vol. 08.02 Committee D20
$86.00
In stock
Significance and Use
5.1 The OIT is a qualitative assessment of the level (or degree) of stabilization of the material tested. This test has the potential to be used as a quality control measure to monitor the stabilization level in formulated resin as received from a supplier, prior to extrusion.
Note 2:The OIT measurement is an accelerated thermal-aging test and as such can be misleading. Caution should be exercised in data interpretation since oxidation reaction kinetics are a function of temperature and the inherent properties of the additives contained in the sample. For example, OIT results are often used to select optimum resin formulations. Volatile antioxidants may generate poor OIT results even though they may perform adequately at the intended use temperature of the finished product.
Note 3:There is no accepted sampling procedure, nor have any definitive relationships been established for comparing OIT values on field samples to those on unused products, hence the use of such values for determining life expectancy is uncertain and subjective.
Scope
1.1 This test method outlines a procedure for the determination of oxidative-induction time (OIT) of polymeric materials by differential scanning calorimetry (DSC). It is applicable to polyolefin resins that are in a fully stabilized/compounded form.
1.2 The values stated in SI units are to be regarded as the standard.
1.3This standard does not purport to address all of the safety concerns, if any, associated with its use. It is the responsibility of the user of this standard to establish appropriate safety and health practices and determine the applicability of regulatory limitations prior to use. Specific hazards information is given in Section 8.
Note 1:This standard and ISO 11357–6 2013 address the same subject matter, but differ in technical content.
Domestic orders are delivered via United Parcel Service (UPS) or United States Postal Service (USPS). Transit
times average 3 to 5 business days. Please be aware that UPS will not deliver packages to Post Office Boxes.
International orders are delivered via courier post services which can be either a postal service, courier
service, or a combination of both. Standard Service is untraceable. Please allow 4-7 weeks for delivery.
Please be aware that carriers will not deliver packages to Post Office Boxes. Because of the variability of
customs processes and procedures in different countries, ASTM International cannot guarantee transit times to
international destinations. Customs duty and taxes are the responsibility of the consignee.
Shipping & Handling charges follow the rate schedule, below:
Order Total
Shipping & Handling Fee (US Domestic)
Up to $50.00
$18.72
$50.01 to $100.00
$20.80
$100.01 to $150.00
$29.52
$150.01 to $250.00
$39.09
$250.01 to $500.00
$56.25
$500.01 to $750.00
$76.42
$750.01 to $1000.00
$93.15
$1000.01 to $1500.00
$121.27
$1500.01 to $2500.00
$158.38
$2500.01 to $4999.00
$209.04
$5000.00 to higher
FREE
Order Total
Shipping & Handling Fee (International)
Up to $50.00
$68.72
$50.01 to $100.00
$70.80
$100.01 to $150.00
$79.52
$150.01 to $250.00
$89.09
$250.01 to $500.00
$106.25
$500.01 to $750.00
$126.42
$750.01 to $1000.00
$143.15
$1000.01 to $1500.00
$171.27
$1500.01 to $2500.00
$208.38
$2500.01 to $4999.00
$259.04
$5000.00 to higher
FREE
Shipping and Handling charges are approximate. Additional charges may be incurred if your order requires multiple shipments. This does not apply to complete sets and sections.