Standard Test Methods and Practices for Evaluating Physical and Chemical Properties of Particulate Ion-Exchange Resins (Withdrawn 2026)
Standard Test Methods and Practices for Evaluating Physical and Chemical Properties of Particulate Ion-Exchange Resins (Withdrawn 2026)D2187-17ASTM|D2187-17|en-USStandard Test Methods and Practices for Evaluating Physical and Chemical Properties of Particulate Ion-Exchange Resins (Withdrawn 2026)StandardD2187 Standard Test Methods and Practices for Evaluating Physical and Chemical Properties of Particulate Ion-Exchange Resins (Withdrawn 2026)>newBOS Vol. 11.02 Committee D19
$0.00
Out of stock
ASTM International
Significance and Use
7.1 The ionic form of an ion-exchange material affects both its equivalent mass and its equilibrium water content. These in turn influence the numerical values obtained in exchange capacity determinations, in density measurements, and in the size of the particles. To provide a uniform basis for comparison, therefore, the sample should be converted to a known ionic form before analysis. This procedure provides for the conversion of cation-exchange materials to the sodium form and anion-exchange materials to the chloride form prior to analysis. These forms are chosen since they permit samples to be weighed and dried without concern for air contamination or decomposition. If other ionic forms are used this fact should be noted in reporting the results.
Scope
1.1 These test methods cover the determination of the physical and chemical properties of ion-exchange resins when used for the treatment of water. They are intended for use in testing both new and used materials. The following thirteen test methods are included:
Sections
Test Practice A—Pretreatment
6 – 10
Test Method B—Water Retention Capacity
11 – 18
Test Method C—Backwashed and Settled Density
19 – 26
Test Method D—Particle Size Distribution
27 – 35
Test Method E—Salt-Splitting Capacity of Cation-Exchange Resins
36 – 45
Test Method F—Total Capacity of Cation-Exchange Resins
46 – 55
Test Method G—Percent Regeneration of Hydrogen-Form Cation-Exchange Resins
56 – 64
Test Method H—Total and Salt-Splitting Capacity of Anion-Exchange Resins
65 – 73
Test Practice I—Percent Regeneration of Anion Exchange Resins
74 – 82
Test Practice J—Ionic Chloride Content of Anion-Exchange Resins
83 – 90
Test Method K—Carbonate Content of Anion-Exchange Resins
91 – 99
Test Method L—Sulfate Content of Anion Exchange Resins
100 – 108
Test Practice M—Total Anion Capacity of Anion-Exchange Resins
109 – 117
1.2 The values stated in SI units are to be regarded as standard. The values given in parentheses are mathematical conversions to inch-pound units that are provided for information only and are not considered standard.
1.3This standard does not purport to address all of the safety concerns, if any, associated with its use. It is the responsibility of the user of this standard to establish appropriate safety, health and environmental practices and determine the applicability of regulatory limitations prior to use. Specific precautionary statements are given in Section 10.8.
1.4This international standard was developed in accordance with internationally recognized principles on standardization established in the Decision on Principles for the Development of International Standards, Guides and Recommendations issued by the World Trade Organization Technical Barriers to Trade (TBT) Committee.
Language unavailable
Format unavailable
What is a Redline?
Why Redline?
A PDF redline is a quick and easy way to compare all of the changes between the current, active standard and the previous version.
With a redline you'll immediately see:
additions
deletions
and other changes between the two standards.
Save Time and Trouble!With a Redline you no longer have to spend time trying to determine what has changed in the new standard! Redlines save you time and ensure you see what the changes are to the standard.
PriceWhen you select the "Standard + Redline" option you get both documents! Best of all, the cost of a Standard + Redline is only slightly more than buying the Active Standard by itself.
Domestic orders are delivered via United Parcel Service (UPS) or United States Postal Service (USPS). Transit
times average 3 to 5 business days. Please be aware that UPS will not deliver packages to Post Office Boxes.
International orders are delivered via courier post services which can be either a postal service, courier
service, or a combination of both. Standard Service is untraceable. Please allow 4-7 weeks for delivery.
Please be aware that carriers will not deliver packages to Post Office Boxes. Because of the variability of
customs processes and procedures in different countries, ASTM International cannot guarantee transit times to
international destinations. Customs duty and taxes are the responsibility of the consignee.
Shipping & Handling charges follow the rate schedule, below:
Order Total
Shipping & Handling Fee (US Domestic)
Up to $50.00
$18.72
$50.01 to $100.00
$20.80
$100.01 to $150.00
$29.52
$150.01 to $250.00
$39.09
$250.01 to $500.00
$56.25
$500.01 to $750.00
$76.42
$750.01 to $1000.00
$93.15
$1000.01 to $1500.00
$121.27
$1500.01 to $2500.00
$158.38
$2500.01 to $4999.00
$209.04
$5000.00 to higher
FREE
Order Total
Shipping & Handling Fee (International)
Up to $50.00
$68.72
$50.01 to $100.00
$70.80
$100.01 to $150.00
$79.52
$150.01 to $250.00
$89.09
$250.01 to $500.00
$106.25
$500.01 to $750.00
$126.42
$750.01 to $1000.00
$143.15
$1000.01 to $1500.00
$171.27
$1500.01 to $2500.00
$208.38
$2500.01 to $4999.00
$259.04
$5000.00 to higher
FREE
Shipping and Handling charges are approximate. Additional charges may be incurred if your order requires multiple shipments. This does not apply to complete sets and sections.