SYMPOSIA PAPER
Published:
01 January 1985
STP28971S
Damage Threshold of Fused Silica at 3ωo
SourceOur laser-matter interaction program requires the conversion of our OCTAL laser from 1.06 μm to 0.355 μm. Fused silica is used to realized the focusing lens and the last optics (KDP windows, debris-shield, etc). A damage test facility at 3ωo was build in CEA Limeil in order to compare the performance of the different French manufacturers production (polished fused silica was provided by SORO, REOSC, BERTIN ESO, STIGMA-OPTIQUE, ELECTRO-QUARTZ).
Author Information
Mengue, JF
Friart, D
Related
Reprints and Permissions
Details
Developed by Committee: F01
Pages: 179–182
DOI: 10.1520/STP28971S
ISBN-EB: 978-0-8031-4956-4
ISBN-13: 978-0-8031-0930-8