SYMPOSIA PAPER
Published:
01 January 1986
STP23123S
Pulse Duration Dependence of 1064-nm Laser Damage Thresholds of Porous Silica Antireflection Coatings on Fused Silica Substrates
SourceWe used 1064-nm pulses with durations of 1, 5, 9 ns to measure laser-damage thresholds of 10 porous silica antireflection coatings deposited from both methanol and ethanol solutions containing silica particles with diameters of 10–20 nm. The median thresholds measured at the three pulse durations, 10.8 J/cm2, 26.5 J/cm2, and 38 J/cm2, scaled as pulse duration to the 0.56 power.
Author Information
Milam, D
Lawrence Livermore National Laboratory, Livermore, CA
Thomas, IM
Lawrence Livermore National Laboratory, Livermore, CA
Weinzapfel, C
Lawrence Livermore National Laboratory, Livermore, CA
Wilder, JG
Lawrence Livermore National Laboratory, Livermore, CA
Related
Reprints and Permissions
Details
Developed by Committee: F01
Pages: 211–216
DOI: 10.1520/STP23123S
ISBN-EB: 978-0-8031-4997-7
ISBN-13: 978-0-8031-0960-5