Standard Test Methods of Polyurethane Raw Materials: Determination of the Polymerized Ethylene Oxide Content of Polyether PolyolsD4875-05ASTM|D4875-05|en-USStandard Test Methods of Polyurethane Raw Materials: Determination of the Polymerized Ethylene Oxide Content of Polyether PolyolsStandardD4875 Standard Test Methods of Polyurethane Raw Materials: Determination of the Polymerized Ethylene Oxide Content of Polyether Polyols>newBOS Vol. 08.02 Committee D20
$86.00
In stock
Significance and Use
Measurements of EO content correlate with polyol reactivity (as related to primary hydroxyl content), linearity of foam rise, and the hydrophilicity of the polyol and final product.
Statistical data suggest that the 13C NMR test method is the preferred method for measuring low levels (less than 10 %) of polymerized EO in polyols.
The 1H and 13C NMR test methods give different results which are highly correlated. The equation of the linear regression is:
The standard deviation of the regression is 0.49 and the multiple R-square is 0.9990.
Scope
1.1 Test Method A—Proton Nuclear Magnetic Resonance Spectroscopy (1H NMR) measures polymerized ethylene oxide (EO) in ethylene oxide-propylene oxide polyethers used in flexible urethane foams and nonfoams. It is suitable for diols made from the commonly used initators and containing EO percentages above five. For triols initiated with glycerin and trimethylol propane, an uncorrected EO value is obtained since both initiators have protons that contribute to the EO measurement.
1.2 Test Method B—Carbon-13 Nuclear Magnetic Resonance Spectroscopy (13C NMR) measures the polymerized EO content of ethylene oxide-propylene oxide polyethers used in flexible urethane foams and nonfoams. It is suitable for diols and triols made from the commonly used initiators and containing EO percentages above five.
Note 1—There are no equivalent ISO standards.
1.3 This standard does not purport to address all of the safety concerns, if any, associated with its use. It is the responsibility of the user of this standard to establish appropriate safety and health practices and determine the applicability of regulatory limitations prior to use.
Domestic orders are delivered via United Parcel Service (UPS) or United States Postal Service (USPS). Transit
times average 3 to 5 business days. Please be aware that UPS will not deliver packages to Post Office Boxes.
International orders are delivered via courier post services which can be either a postal service, courier
service, or a combination of both. Standard Service is untraceable. Please allow 4-7 weeks for delivery.
Please be aware that carriers will not deliver packages to Post Office Boxes. Because of the variability of
customs processes and procedures in different countries, ASTM International cannot guarantee transit times to
international destinations. Customs duty and taxes are the responsibility of the consignee.
Shipping & Handling charges follow the rate schedule, below:
Order Total
Shipping & Handling Fee (US Domestic)
Up to $50.00
$18.72
$50.01 to $100.00
$20.80
$100.01 to $150.00
$29.52
$150.01 to $250.00
$39.09
$250.01 to $500.00
$56.25
$500.01 to $750.00
$76.42
$750.01 to $1000.00
$93.15
$1000.01 to $1500.00
$121.27
$1500.01 to $2500.00
$158.38
$2500.01 to $4999.00
$209.04
$5000.00 to higher
FREE
Order Total
Shipping & Handling Fee (International)
Up to $50.00
$68.72
$50.01 to $100.00
$70.80
$100.01 to $150.00
$79.52
$150.01 to $250.00
$89.09
$250.01 to $500.00
$106.25
$500.01 to $750.00
$126.42
$750.01 to $1000.00
$143.15
$1000.01 to $1500.00
$171.27
$1500.01 to $2500.00
$208.38
$2500.01 to $4999.00
$259.04
$5000.00 to higher
FREE
Shipping and Handling charges are approximate. Additional charges may be incurred if your order requires multiple shipments. This does not apply to complete sets and sections.