Standard Specification for Steel, Sheet and Strip, High-Strength, Low-Alloy, Columbium or Vanadium, or Both, Hot-Rolled and Cold-Rolled (Withdrawn 2000)A0607-98ASTM|A0607-98|en-USStandard Specification for Steel, Sheet and Strip, High-Strength, Low-Alloy, Columbium or Vanadium, or Both, Hot-Rolled and Cold-Rolled (Withdrawn 2000)StandardA607 Standard Specification for Steel, Sheet and Strip, High-Strength, Low-Alloy, Columbium or Vanadium, or Both, Hot-Rolled and Cold-Rolled (Withdrawn 2000)>newBOS Vol. 01.03 Committee A01
$0.00
Out of stock
Scope
1.1 This specification covers high-strength, low-alloy columbium, or vanadium hot-rolled sheet and strip, or cold-rolled sheet, or combinations thereof, in either cut lengths or coils, intended for applications where greater strength and savings in weight are important. The material is available as two classes. They are similar in strength level except that Class 2 offers improved weldability and more formability than Class 1. Atmospheric corrosion resistance of these steels is equivalent to plain carbon steels. With copper specified, the atmospheric corrosion resistance is twice that of plain carbon steel.
1.2 The value stated in inch-pound units are to be regarded as the standard.
1.3 Class 1 material was previously A607 without a class designation.
Language unavailable
Format unavailable
What is a Redline?
Why Redline?
A PDF redline is a quick and easy way to compare all of the changes between the current, active standard and the previous version.
With a redline you'll immediately see:
additions
deletions
and other changes between the two standards.
Save Time and Trouble!With a Redline you no longer have to spend time trying to determine what has changed in the new standard! Redlines save you time and ensure you see what the changes are to the standard.
PriceWhen you select the "Standard + Redline" option you get both documents! Best of all, the cost of a Standard + Redline is only slightly more than buying the Active Standard by itself.
Domestic orders are delivered via United Parcel Service (UPS) or United States Postal Service (USPS). Transit
times average 3 to 5 business days. Please be aware that UPS will not deliver packages to Post Office Boxes.
International orders are delivered via courier post services which can be either a postal service, courier
service, or a combination of both. Standard Service is untraceable. Please allow 4-7 weeks for delivery.
Please be aware that carriers will not deliver packages to Post Office Boxes. Because of the variability of
customs processes and procedures in different countries, ASTM International cannot guarantee transit times to
international destinations. Customs duty and taxes are the responsibility of the consignee.
Shipping & Handling charges follow the rate schedule, below:
Order Total
Shipping & Handling Fee (US Domestic)
Up to $50.00
$18.72
$50.01 to $100.00
$20.80
$100.01 to $150.00
$29.52
$150.01 to $250.00
$39.09
$250.01 to $500.00
$56.25
$500.01 to $750.00
$76.42
$750.01 to $1000.00
$93.15
$1000.01 to $1500.00
$121.27
$1500.01 to $2500.00
$158.38
$2500.01 to $4999.00
$209.04
$5000.00 to higher
FREE
Order Total
Shipping & Handling Fee (International)
Up to $50.00
$68.72
$50.01 to $100.00
$70.80
$100.01 to $150.00
$79.52
$150.01 to $250.00
$89.09
$250.01 to $500.00
$106.25
$500.01 to $750.00
$126.42
$750.01 to $1000.00
$143.15
$1000.01 to $1500.00
$171.27
$1500.01 to $2500.00
$208.38
$2500.01 to $4999.00
$259.04
$5000.00 to higher
FREE
Shipping and Handling charges are approximate. Additional charges may be incurred if your order requires multiple shipments. This does not apply to complete sets and sections.